Sign In | Join Free | My components-electronic.com |
|
Brand Name : BWIN
Model Number : 22ER 6.0ISO
Place of Origin : China
MOQ : 10pcs/box
Price : Negotiable
Payment Terms : T/T, Western Union
Supply Ability : 1-10000pcs 7days
Delivery Time : 7 work days
Packaging Details : Plastic box
Product name : 22ER ISO Carbide Threading Inserts
Material : Carbide Threading Insert
Workpiece : Steel/Stainless steel/Cast iron
Usage : CNC Tool
Color : Black Coated
Coating : PVD/CVD
Hardness : HRC40-HRC60
Feature : High Bending Strength
Application : Machining
Package : 10pcs/Box
Quick Detail:
Description:
22ER 6.0 ISO carbide turning tool is made of high-quality tungsten steel alloy, with high overall hardness, wear resistance and durability, smooth and polished surface, and effective corrosion resistance; Single sided hexagon can be used, cutting is sharp, spiral groove is finely ground, cutting resistance is reduced, cutting is stable and there is no chip accumulation, the generation of chip accumulation tumor and tool clamping are avoided, and efficient machining is realized.
Specifications:
Brand | BWIN |
Model | 22ER 22IR |
Color | Black Coated |
Workpiece | Steel/Cast iron/Stainless steel |
Type | Cnc Carbide Threading Insert |
Material | Tungsten Carbide Treading Insert |
Processing Type | Medium Cutting |
Feature | Good process performance |
High efficiency | |
Fine cutting | |
Low friction coefficient | |
High bending strength | |
Standard | ISO |
Quantity | 10pcs/box |
Weight | 0.015kg |
Package | Plastic Box |
Customized Support | OEM, ODM |
Lead Time:
antity(pieces) | 1 - 3000 | >3000 |
Lead time (days) | 7 | To be negotiated |
Notice:
Applications:
Our carbide threading insert could to be processed Alloy steel, Tool steel, carbon steel, stainless steel, Cast iron and Titanium alloy. Working material as following:
1. Rear cutter face wear: (This is a common practical form)
Influence: the workpiece size gradually changes or the surface light intensity decreases
Cause: The linear speed is too high, reaching the service life of the tool
Measures: Adjust the processing parameters, such as reducing the linear speed and using a blade with higher wear resistance
2. Blade breakage: (bad actual effect form)
Effect: sudden change of workpiece size or surface smoothness, resulting in burrs on the spark surface
Cause: Improper parameter setting, improper tool face material selection, poor workpiece rigidity, unstable blade clamping Measures: check whether the parameter setting is reasonable, and select the corresponding tool according to the workpiece material
3. Serious fracture: (very bad actual effect form)
Effect: sudden and unexpected occurrence, resulting in scrapping of tool handle materials or defective and scrapped workpieces
Cause: The processing parameters are set incorrectly, and the vibrating tool workpiece or blade is not installed in place
Measures: set reasonable parameters, reduce the feed rate and chip, select the corresponding processing blade, and strengthen the rigidity of the workpiece and blade
4. Chips:
Effect: the size of the workpiece is inconsistent, the surface finish is poor, and the workpiece surface is attached with fluff or burrs. Cause: the cutting speed is too low, the feed is too low, and the blade is not sharp enough
Measures: improve the cutting speed, and use blades with higher sharpness for feed rate
![]() |
22er Carbide Threading Inserts 22ir 6.0 ISO 60 Degree For CNC Tool Images |